Application:
Used for matrices, foundry patterns, casted handworks. High toughness. For pilot moulds for vacuum forming moulds.
Processing methods:
Face and solid casting also at high thickness using the filled product. The working time allows to realize parts of medium-large size.
Further casting can be made by successive application on the previous gelled layer (within 10 mins). The greater the filler loading, the lower the shrinkage. Medium-fast curing.
Attention:
Homogenize the resin before use (follow the instructions).
Description:
Two component odourless system. The filler can be added in the suggested ratio or in a different ratio depending on the application and on the required thickness. Very high quality of reproduction. Low exothermic peak. Low shrinkage. The use of EF 31 filler (mix ratio 100:100:150) allows production of components with lower specific weight.